Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC BC 110 Crystalline Polyethylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer SABIC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC BC 110 Crystalline Polyethylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: BC 110 is a crystalline, high molecular weight thermoplastic polymer made by a continuous melt-phase polymerization process followed by solid-state polymerization.Characteristics: BC 110 is a specially formulated bottle grade PET that is characterized by medium I.V.Typical Applications: BC 110 is especially suitable for the production of bottles for carbonated drinks in temperate climates. It can also be used for bottles for general packaging applications, e.g., edible oil & thermoformed packaging.Information provided by SABIC.
Physical Properties Metric English Comments
Bulk Density 0.828 - 0.848 g/cc
0.0299 - 0.0306 lb/in³
ASTM D1895
Density <= 1.39 g/cc
<= 0.0502 lb/in³
crystalline density; SABIC (IRC0032)
Viscosity Test 78 - 82 cm³/g
78 - 82 cm³/g
Intrinsic; SABIC (IRC0041)
Maximum Moisture Content <= 0.35
<= 0.35
% w/w; SABIC (IRC0050)
Thermal Properties Metric English Comments
Melting Point 246 - 256 °C
475 - 493 °F
SABIC (IRC0053)
Chemical Properties Metric English Comments
Acetaldehyde <= 1.00 ppm
<= 1.00 ppm
SABIC (IRC0057)
Descriptive Properties Value Comments
Color (b) -1.5 ± 2.0
Color (L) 89 ± 4.0
DEG Content < 1.5 % w/w
SABIC (IRC0055)
Dust Content < 0.01 % w/w
SABIC (IRC0060)