Material Notes:
LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Water Absorption 0.040 %

@Time 86400 sec
0.040 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 260 MPa
37700 psi
5 mm/min; ISO 527
Elongation at Break 1.5 %
1.5 %
5 mm/min; ISO 527
2.5 %
2.5 %
Flexural Strain, break, 2 mm/min; ISO 178
Tensile Modulus 25.7 GPa
3730 ksi
1 mm/min; ISO 527
Flexural Yield Strength 359 MPa
52100 psi
2 mm/min; ISO 178
Flexural Modulus 19.1 GPa
2770 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 520 µm/m-°C

@Temperature 23.0 - 60.0 °C
289 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
31.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257