| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP LUBRICOMP |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.50 g/cc | 0.0542 lb/in³ | ISO 1183 |
| 1.50 g/cc | 0.0542 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.120 % | 0.120 % | 23°C / 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ISO 294 |
| 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 | |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ASTM D955 |
| 0.0040 - 0.0060 cm/cm @Time 86400 sec |
0.0040 - 0.0060 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 88.0 MPa | 12800 psi | ASTM D638 |
| 98.0 MPa | 14200 psi | ISO 527 | |
| Elongation at Break | 2.4 % | 2.4 % | ASTM D638 |
| 3.4 % | 3.4 % | ISO 527 | |
| Tensile Modulus | 6.52 GPa | 946 ksi | 50 mm/min; ASTM D638 |
| 7.22 GPa | 1050 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 146 MPa | 21200 psi | ISO 178 |
| 151 MPa | 21900 psi | ASTM D790 | |
| Flexural Modulus | 5.83 GPa | 846 ksi | ISO 178 |
| 5.87 GPa | 851 ksi | ASTM D790 | |
| Izod Impact, Notched | 1.06 J/cm | 1.99 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 5.01 J/cm | 9.39 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 40.0 kJ/m² | 19.0 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 12.0 J | 8.85 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.42 | 0.42 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.34 | 0.34 | ASTM D3702 Modified |
| K (wear) Factor | 232 x 10<sup>-8</sup> mm³/N-M | 115 x 10<sup>-10</sup> in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 20.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 61.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 61.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
34.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 138 °C | 280 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 137 °C @Thickness 3.20 mm |
279 °F @Thickness 0.126 in |
unannealed; ASTM D648 |