SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
1.473 g/cc
0.05322 lb/in³
ASTM D792
Moisture Absorption 0.210 %
0.210 %
50% RH, 24 hrs; ASTM D570
0.320 %
0.320 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ASTM D955
0.0070 - 0.0090 cm/cm

@Time 86400 sec
0.0070 - 0.0090 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 74.0 MPa
10700 psi
ISO 527
77.0 MPa
11200 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ISO 527
1.1 %
1.1 %
ASTM D638
Tensile Modulus 10.17 GPa
1475 ksi
1 mm/min; ISO 527
10.2 GPa
1480 ksi
50 mm/min; ASTM D638
Flexural Strength 106 MPa
15400 psi
ISO 178
114 MPa
16500 psi
ASTM D790
Flexural Modulus 7.14 GPa
1040 ksi
ASTM D790
8.27 GPa
1200 ksi
ISO 178
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.28 J/cm
2.40 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 7.00 J
5.16 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 4.00 J
2.95 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702 Modified
Coefficient of Friction, Static 0.31
0.31
ASTM D3702 Modified
K (wear) Factor 407 x 10-8 mm³/N-M
202 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
66.0 °C

@Thickness 3.20 mm
151 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10 - 10000 ohm-cm
10 - 10000 ohm-cm
ASTM D257
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D257