PPE/HIPS unfilled for auto application
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 9.3 g/10 min

@Load 10.0 kg,
Temperature 250 °C
9.3 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
SABIC - Japan Method
Elongation at Break 108 %
108 %
SABIC - Japan Method
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 0.200 GPa
29.0 ksi
ASTM D790
Izod Impact, Notched 2.27 J/cm
4.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
38.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 116 °C

@Thickness 6.40 mm
241 °F

@Thickness 0.252 in
unannealed; ASTM D648