S&E Specialty Polymers GTPO8290FR-75 RoHS PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GTPO8290FR-75 RoHS PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: RoHS compliant, flexible flame retardant thermoplastic olefin compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength 12.4 MPa
1800 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature <= -45.0 °C
<= -49.0 °F
ASTM D746
Oxygen Index 25 %
25 %
ASTM D2863
Descriptive Properties Value Comments
Color <26 L
Colorimeter