| Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber |
| Manufacturer | Seals Eastern, Inc |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Seals Eastern 5400 Nitrile Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D297, 15 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 40 | >= 40 | ASTM D2240, Type A |
| 50 | 50 | AVG; ASTM D2240, Type A | |
| Tensile Strength at Break | >= 8.811 MPa | >= 1278 psi | ASTM D412 Method A |
| 13.26 MPa | 1923 psi | AVG; ASTM D412 Method A | |
| Tensile Strength, Yield | >= 0.448 MPa | >= 65.0 psi | Stress at Elongation M50; ASTM D412 Method A |
| 0.531 MPa | 77.0 psi | AVG Stress at Elongation M25; ASTM D412 Method A | |
| >= 0.579 MPa | >= 84.0 psi | Stress at Elongation M100; ASTM D412 Method A | |
| 0.614 MPa | 89.0 psi | AVG Stress at Elongation M50; ASTM D412 Method A | |
| 0.820 MPa | 119 psi | AVG Stress at Elongation M100; ASTM D412 Method A | |
| Elongation at Break | >= 653 % | >= 653 % | ASTM D412 Method A |
| 900 % | 900 % | AVG; ASTM D412 Method A | |
| Modulus of Elasticity | 0.00357 GPa | 0.518 ksi | ASTM D412 Method A |
| Shear Modulus | 0.00119 GPa | 0.173 ksi | ASTM D412 Method A |
| Secant Modulus | 0.00336 GPa | 0.487 ksi | ASTM D412 Method A |
| Tear Strength Test | 191 | 191 | (psi); ASTM D624, Die B |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glass Transition Temp, Tg | -29.4 °C | -21.0 °F | ASTM D1329 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Strain Energy / Unit Volume at 20% Elongation (psi) | 8 |