Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH 3462 Polypropylene, Extrusion Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3462 Polypropylene, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Homopolymer extrusion grade for slit film and fibrillated tapesProcess Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.FDA - FINA 3462 complies with all applicable FDA regulations for food contact applications.Recommended Applications -- FINA 3462 is recommended for slit film monofilament and fibrillated tape applications requiring improved process stability.Processing - FINA 3462 processes on conventional extrusion equipment with typical melt temperatures of 400-500°F (204-260°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 4.1 g/10 min
4.1 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D288A
Hardness, Shore D 80
80
ASTM D1706
Tensile Strength, Ultimate 34.5 MPa
5000 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Modulus of Elasticity 1.515 GPa
219.7 ksi
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.317 J/cm
0.594 ft-lb/in
ASTM D256A
Izod Impact, Unnotched 9.00 J/cm
16.9 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 200 - 260 °C
392 - 500 °F
Extrusion