Silberline SilBerCote® 3650-20Y

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name SilBerCote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline SilBerCote® 3650-20Y.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts additional detergent resistance and adhesion properties versus the SilBerCote® Z series. SilBerCote® Y is typically formulated into liquid coatings for plastic substrates (automotive interior and consumer electronics applications).Applications: General Industrial
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
Bulk Factor 0.104
0.104
Volatiles 50 %
50 %
Particle Size 16 µm
16 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
1% retained
Descriptive Properties Value Comments
Solvents Mineral Spirits