Solvay RHODAPHOSE® DIPHENYL PHOSPHATE DIHYDRATE Phosphorus Derivative

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODAPHOSE® DIPHENYL PHOSPHATE DIHYDRATE Phosphorus Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Identification: DIPHENYL PHOSPHATE DIHYDRATECAS: 838 – 85 – 7EC: 212 – 657 – 2Available in: Asia Pacific, Europe, Latin America and North America Solubility: Organic Solvents. Soluble in alcohol (ethanol)Applications: RHODAPHOS® DIPHENYL PHOSPHATE DIHYDRATE is a pharmaceutical intermediate. It finds use in: Selective manufacturing of phosphoric acid diesters and Protective agent for hydroxyl groups.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.590 g/cc
0.0213 lb/in³
Thermal Properties Metric English Comments
Melting Point 38.0 - 48.0 °C
100 - 118 °F
Boiling Point 127 °C
261 °F
Processing Properties Metric English Comments
Moisture Content 10.5 - 14.5 %
10.5 - 14.5 %
AM6378
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White to off white lumpy powder or aggregates
Composition DI-phenyl phosphate
98%, AM6310
TPP
<1%, AM6310