Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or steam at high temperature. Catalyst PS/2 UV contains a processing aid and UV stabilization.Features: Antioxidant; Good Thermal Aging Resistance; Good UV ResistanceUses: Piping; Plumbing Parts; Potable Water ApplicationsAdditional Properties: Extruder Screw Compression Ratio - >2.5:1; Extruder Screw L/D Ratio - 25:1 to 30:1; Head Temperature - 200 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Apparent Bulk Density 0.550 g/cc
0.0199 lb/in³
ASTM D1895
Melt Flow 0.80 g/10 min
0.80 g/10 min
ISO 1133
Processing Properties Metric English Comments
Zone 1 150 - 200 °C
302 - 392 °F
Zone 2 150 - 200 °C
302 - 392 °F
Zone 3 150 - 200 °C
302 - 392 °F
Zone 4 150 - 200 °C
302 - 392 °F
Zone 5 150 - 200 °C
302 - 392 °F
Die Cooling Temperature 210 °C
410 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Processing Technique Extrusion; Pipe Extrusion
Users viewing this material also viewed the following: