| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accucomp ABS ABS892EL High Heat Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | MD; ASTM D955 |
| Melt Flow | 0.60 g/10 min | 0.60 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 106 | 106 | ASTM D785 |
| Tensile Strength at Break | 42.0 MPa | 6090 psi | ASTM D638 |
| Tensile Strength, Yield | 51.0 MPa | 7400 psi | ASTM D638 |
| Elongation at Break | 12 % | 12 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
| Flexural Strength | 71.98 MPa | 10440 psi | ASTM D790 |
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
| Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |
UL File #E56070 |