Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Solvay Specialty Polymers
Trade Name Cogegum®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution; furthermore, toxic and corrosive gases emission and smoke generation are particularly reduced. These characteristics make this compound suitable in all applications where the fire behavior of cable materials is one of the main concerns to be considered in establishing a high safety level in public places. This material complies with RoHS requirements.Features: Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 20-25 L/D ratio are suggested), and an adequate barrel thermoregulation.Additional Properties: Bending Test - IEC 60811 (-25°C): Pass; Calorific Potential - ISO 1716 15.7 MJ/kg; Cold Impact - IEC 60811 (-25°C): Pass; Collar Temperature - 150 to 170 °C; Corrosive Gas in Smoke - IEC 60754-2 < 10.0 µS/mm; Corrosive Gas in Smoke - IEC 60754-2 > 4.30; Halogenidric Acid Emissions - IEC 60754-1 < 0.10 %; Head Temperature - 150 to 170 °C; Heat Shock - IEC 60811 (150°C): Pass; Hot Pressure Test - IEC 60811 (90°C): < 50 %; Insulation Resistance Constant - IEC 60502 (20°C): 800 Mohm·km; Insulation Resistance Constant - IEC 60502 (70°C): 10 Mohm·km; Temperature Index (Burning) - NES 715 300 °C; Water Absorption - IEC 60811 (100°C): 2.20 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded, 10% Igepal; ASTM D1693
Melt Flow 5.1 g/10 min

@Load 21.6 kg,
Temperature 150 °C
5.1 g/10 min

@Load 47.6 lb,
Temperature 302 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ISO 868
Tensile Strength at Break 12.3 MPa
1780 psi
ASTM D638
Elongation at Break 190 %
190 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 39 %
39 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 2.60e+12 ohm-cm

@Temperature 70.0 °C
2.60e+12 ohm-cm

@Temperature 158 °F
ASTM D257
2.20e+14 ohm-cm

@Temperature 20.0 °C
2.20e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Processing Properties Metric English Comments
Zone 1 130 - 150 °C
266 - 302 °F
Zone 2 130 - 160 °C
266 - 320 °F
Zone 3 140 - 160 °C
284 - 320 °F
Zone 4 140 - 160 °C
284 - 320 °F
Die Cooling Temperature 150 - 180 °C
302 - 356 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved