Material Notes:
Hylar® 301F is a high melt viscosity polyvinylidene fluoride (PVDF) powder used for non-architectural dispersion coatings.Features: High Viscosity; HomopolymerUses: Coating ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 44.0 J/g; Heat of Fusion - ASTM D3418 40.0 J/g; Hegman Grind - ASTM D1210 5.50; Thermal Stability - 375 °C; Thermal Stability - 410 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.75 - 1.77 g/cc
0.0632 - 0.0639 lb/in³
ASTM D1505
Water Absorption at Saturation 0.020 %
0.020 %
ASTM D570
Viscosity 2.90e+6 - 3.30e+6 cP
2.90e+6 - 3.30e+6 cP
Melt Viscosity; ASTM D3835
Thermal Properties Metric English Comments
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
ASTM C351
Melting Point 160 °C
320 °F
DSC
Crystallization Temperature 124 °C
255 °F
Peak; ASTM D3418
Optical Properties Metric English Comments
Gloss 25 %
25 %
60°; ASTM D2457
Descriptive Properties Value Comments
Availability Europe; North America
Form Powder
Processing Technique Coating