Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer Solvay Specialty Polymers
Trade Name Ixef®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; High Flow; High Stiffness; High Strength; Impact Modified; Low Moisture Absorption; Outstanding Surface FinishUses: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Business Equipment; Camera Applications; Electrical Housing; Electrical/Electronic Applications; Furniture; Gears; Housings; Industrial Applications; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other ToolsInjection Molding Notes: Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Dry; ISO 1183
Filler Content 50 %
50 %
Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength, Yield 200 MPa
29000 psi
ISO 527-2
Elongation at Break 2.7 %
2.7 %
ISO 527-2
Tensile Modulus 16.0 GPa
2320 ksi
ISO 527-2
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Melt Temperature 270 °C
518 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 120 °C

@Time 1800 - 5400 sec
248 °F

@Time 0.500 - 1.50 hour
Descriptive Properties Value Comments
Additive Impact Modifier
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Colors; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant