Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS); Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics: High temperatureNon-stickCorrosion resistantApplications: CoatingsInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line.
Physical Properties Metric English Comments
Particle Mesh Size 35 Mesh
35 Mesh
99.8 wt% Passing
60 Mesh
60 Mesh
99.5 wt% Passing
Melt Flow 5000 g/10 min
5000 g/10 min
Ash 0.80 %
0.80 %
Thermal Properties Metric English Comments
Melting Point 316 °C
600 °F
ASTM D1283
Descriptive Properties Value Comments
Color Off White