| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled |
| Manufacturer | Lanxess |
| Trade Name | Pocan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Lanxess Pocan® B 3215 XF 000000 PBT, 10% Glass Fiber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ISO 294-4, 2577 |
| Linear Mold Shrinkage, Transverse | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
| Melt Flow | 44 g/10 min @Load 2.16 kg, Temperature 260 °C |
44 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 80.0 MPa | 11600 psi | ISO 527-1/-2 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1/-2 |
| Tensile Modulus | 4.30 GPa | 624 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | <= 1.00 J/cm² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 180 °C | 356 °F | ISO 75-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 260 °C | 500 °F | Injection Molding; ISO 294 |
| Mold Temperature | 80.0 °C | 176 °F | Injection Molding; ISO 10724 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Form | Pellets | |
| ISO Shortname | ISO 7792-1-PBT,GHPMR,09-040,GF10 | |
| Processing | Injection molding | |