Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Solvera® PT 5071 PFPE Surface Treatment

Category Fluid , Polymer
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Solvera®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Solvera® PT 5071 PFPE Surface Treatment.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solvera® PFPE is a sustainable surface treatment developed to increase the grease resistance of paper packaging, pizza boxes, popcorn bags, pet food bags and food wraps. Both solvent and aqueous formulations are available and can be diluted to any concentration with water. It complies with FDA regulations 21 CFR 176.180 and 21 CFR 176.170 and does not contain perfluoro-octanyl acid (PFOA) and perfluoro-octanyl sulfonate (PFOS) nor is it based on telomer chemistry.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
pH 7.0 - 9.0
7.0 - 9.0
Viscosity <= 100 cP
<= 100 cP
Descriptive Properties Value Comments
Appearance Clear Solution
Dry Content 20 wt. %
Flash Point (°C) None
Solvent Content 5 wt. %
DPM, di-propylene glycol methyl ether
Users viewing this material also viewed the following: