Material Notes:
Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phosphorus flame retardant grade, offers excellent filling qualities and with good mechanical properties. This grade is stabilized to offer a very low migration and corrosion of metallic contacts. It is particularly suitable for molding insulating parts for electrical devices: connectors, contactors, bobbins coil formers and thin parts under stress. This product is available in natural and black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527 Type 1A
Elongation at Break 3.5 %
3.5 %
ISO 527 Type 1A
Tensile Modulus 6.20 GPa
899 ksi
ISO 527 Type 1A
Flexural Strength 155 MPa
22500 psi
ISO 178
Flexural Modulus 5.20 GPa
754 ksi
ISO 178
Charpy Impact Unnotched 7.20 J/cm²
34.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %