| Category | Metal , Nonferrous Metal , Nickel Alloy , Superalloy |
| Manufacturer | Special Metals (includes the former Inco Alloys International Inc.) |
| Trade Name | INCONEL® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Special Metals INCONEL® 601GC® Nickel Superalloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.11 g/cc | 0.293 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 586 - 689 MPa | 85000 - 100000 psi | Annealed temper |
| Tensile Strength, Yield | 207 - 345 MPa @Strain 0.200 % |
30000 - 50000 psi @Strain 0.200 % |
Annealed temper |
| Elongation at Break | 35 - 55 % | 35 - 55 % | Annealed temper |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 0.448 J/g-°C | 0.107 BTU/lb-°F | |
| Melting Point | 1301 - 1368 °C | 2374 - 2494 °F | |
| Solidus | 1301 °C | 2374 °F | |
| Liquidus | 1368 °C | 2494 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Aluminum, Al | 0.80 - 1.7 % | 0.80 - 1.7 % | |
| Carbon, C | <= 1.0 % | <= 1.0 % | |
| Chromium, Cr | 21 - 25 % | 21 - 25 % | |
| Copper, Cu | <= 1.0 % | <= 1.0 % | |
| Iron, Fe | 15 % | 15 % | |
| Manganese, Mn | <= 1.0 % | <= 1.0 % | |
| Nickel, Ni | 58 - 63 % | 58 - 63 % | |
| Nitrogen, N | 0.020 - 0.070 % | 0.020 - 0.070 % | |
| Silicon, Si | <= 1.0 % | <= 1.0 % | |
| Sulfur, S | <= 0.015 % | <= 0.015 % | |
| Zirconium, Zr | 0.070 - 0.25 % | 0.070 - 0.25 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Magnetic Permeability | 1.003 | 1.003 | at 200 Oersted (15.9 kA/m) |
| Curie Temperature | <= -196 °C | <= -321 °F |