Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N220 Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N220 Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N22090.0Coumarone-Indene Resin30.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Mooney Viscosity 62

@Temperature 121 °C
62

@Temperature 250 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Tensile Strength, Yield 30.0 MPa
4350 psi
Elongation at Yield 370 %
370 %
100% Modulus 0.008791 GPa
1.275 ksi
300% Modulus 0.0276 GPa
4.00 ksi
Tear Strength 82.5 kN/m
471 pli
Graves
Abrasion 350
350
NBS Index
Compression Set 31 %
31 %
Method B
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 142 °C
1.00 hour

@Temperature 287 °F