Taiwan Sheen Soon Sheenthane® A9660 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A9660 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 93 - 97
93 - 97
Tensile Strength 34.3 MPa
4980 psi
Elongation at Break 350 %
350 %
100% Modulus 0.01273 GPa
1.846 ksi
300% Modulus 0.0245 GPa
3.56 ksi
Processing Properties Metric English Comments
Processing Temperature 210 - 230 °C
410 - 446 °F