| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Electrafil® J-1200/CF/20 NAT ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 |
| Water Absorption | 0.30 % | 0.30 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.00050 cm/cm | 0.00050 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 103 MPa | 15000 psi | ASTM D638 |
| Elongation at Break | 1.0 % | 1.0 % | ASTM D638 |
| Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
| Flexural Modulus | 11.7 GPa | 1700 ksi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.0 - 10 ohm-cm | 1.0 - 10 ohm-cm | ASTM D648 |
| Surface Resistivity per Square | 10 - 100 ohm | 10 - 100 ohm | ASTM D648 |