| Category | Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler |
| Manufacturer | Techmer ES |
| Trade Name | Plaslube® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Plaslube® J-4/30/TF/13/SI/2 NAT PA6/12.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.42 g/cc | 1.42 g/cc | ASTM D792 |
| Water Absorption | 0.13 % | 0.13 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0020 cm/cm | 0.0020 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Flexural Strength | 197 MPa | 28500 psi | ASTM D790 |
| Flexural Modulus | 8.34 GPa | 1210 ksi | ASTM D790 |
| Compressive Strength | 124 MPa | 18000 psi | ASTM D695 |
| Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 48.6 µm/m-°C @Temperature 20.0 °C |
27.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 199 °C | 390 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |