| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, PTFE Filled |
| Manufacturer | Techmer ES |
| Trade Name | Plaslube® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Plaslube® PC-50/TF/22 BK223 Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Water Absorption | 0.12 % | 0.12 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 109 | 109 | ASTM D785 |
| Tensile Strength at Break | 51.7 MPa | 7500 psi | ASTM D638 |
| Elongation at Break | 40 % | 40 % | ASTM D638 |
| Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
| Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
| Compressive Strength | 62.1 MPa | 9000 psi | ASTM D695 |
| Izod Impact, Notched | 1.76 J/cm | 3.30 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 70.2 µm/m-°C @Temperature 20.0 °C |
39.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 135 °C | 275 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |