| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Techmer ES |
| Trade Name | Plastiblend® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Techmer ES Plastiblend® PC/ABS 8001A.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
| Water Absorption | 0.10 % <br>@Time 86400 sec |
0.10 % <br>@Time 24.0 hour |
ASTM D570 |
| Melt Flow | 8.5 g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C |
8.5 g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F |
ASTM D1238 |
| 19 g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C |
19 g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 115 | 115 | ASTM D785 |
| Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
| Elongation at Break | 150 % | 150 % | ASTM D638 |
| Flexural Yield Strength | 86.2 MPa | 12500 psi | ASTM D790 |
| Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
| Izod Impact, Notched | 6.41 J/cm <br>@Thickness 3.17 mm |
12.0 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 124 °C | 255 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | HB | HB |