| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.31 g/cc | 1.31 g/cc | ASTM D792 |
| Water Absorption | 0.10 % | 0.10 % | 24 hours; ASTM D570 (2) |
| Water Absorption at Saturation | 0.50 % | 0.50 % | ASTM D570 (2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 85 | 85 | ASTM D2240 |
| Tensile Strength, Ultimate | 110 MPa | 16000 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Modulus of Elasticity | 3.45 GPa | 500 ksi | ASTM D638 |
| Flexural Strength | 172 MPa | 25000 psi | ASTM D790 |
| Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
| Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 type "A" |
| Coefficient of Friction | 0.40 | 0.40 | ASTM PTM 55007 |
| K (wear) Factor | 755 x 10<sup>-8</sup> mm³/N-M | 375 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM 55010 |
| Limiting Pressure Velocity | 0.298 MPa-m/sec | 8500 psi-ft/min | 4:1 safety factor |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 46.8 µm/m-°C @Temperature 100 °C |
26.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
| Maximum Service Temperature, Air | 249 °C | 480 °F | |
| Flammability, UL94 | V-0 @Thickness 3.17 mm |
V-0 @Thickness 0.125 in |
ASTM UL-94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.3 @Frequency 1e+6 Hz |
3.3 @Frequency 1e+6 Hz |
ASTM D150 |
| Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
| Dissipation Factor | 0.0030 @Frequency 1e+6 Hz |
0.0030 @Frequency 1e+6 Hz |
ASTM D150 |