| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Technetics Group Amicon™ PET-P
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
| Water Absorption | 0.070 % | 0.070 % | 24 hours; ASTM D570 (2) |
| Water Absorption at Saturation | 0.90 % | 0.90 % | ASTM D570 (2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 87 | 87 | ASTM D2240 |
| Tensile Strength, Ultimate | 85.5 MPa | 12400 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Modulus of Elasticity | 3.17 GPa | 460 ksi | ASTM D638 |
| Flexural Strength | 124 MPa | 18000 psi | ASTM D790 |
| Flexural Modulus | 3.38 GPa | 490 ksi | ASTM D790 |
| Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
| Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 type "A" |
| Coefficient of Friction | 0.20 | 0.20 | ASTM PTM 55007 |
| K (wear) Factor | 121 x 10<sup>-8</sup> mm³/N-M | 60.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM 55010 |
| Limiting Pressure Velocity | 0.0981 MPa-m/sec | 2800 psi-ft/min | 4:1 safety factor |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 59.4 µm/m-°C @Temperature 100 °C |
33.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
| Maximum Service Temperature, Air | 98.9 °C | 210 °F | |
| Flammability, UL94 | HB @Thickness 3.17 mm |
HB @Thickness 0.125 in |
ASTM UL-94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 15.2 kV/mm | 385 kV/in | ASTM D149 |