Material Notes:
Notes: 75°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 75°C FR Plugs Contact Insulators Recognized Component, CSA C22.2 No. 0.6, CSA Flammability Classification: 0.6V-0 at 0.76 mmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore C 70
70
10 seconds; ASTM D2240
Tensile Strength at Break 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 320 %
320 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
UL RTI, Electrical 90.0 °C

@Thickness 0.810 mm
194 °F

@Thickness 0.0319 in
UL 746
90.0 °C

@Thickness 3.00 mm
194 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 90.0 °C

@Thickness 0.810 mm
194 °F

@Thickness 0.0319 in
UL 746
90.0 °C

@Thickness 3.00 mm
194 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 V-0

@Thickness 0.810 mm
V-0

@Thickness 0.0319 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 27 %
27 %
ASTM D2863
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V

@Thickness 3.00 mm
>= 600 V

@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 60 - 120 sec

@Thickness 3.00 mm
60 - 120 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 30 - 60 arcs

@Thickness 3.00 mm
30 - 60 arcs

@Thickness 0.118 in
UL 746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Opaque