Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
ASTM D2240
Tensile Strength, Yield 6.89 MPa
1000 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
300% Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Compression Set 20 %
20 %
23°C, 22 hr.; ASTM D395, Method B