| Category | Metal , Nonferrous Metal , Nickel Alloy , Pure Element |
| Manufacturer | Special Metals (includes the former Inco Alloys International Inc.) |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.91 g/cc | 0.322 lb/in³ | |
| Thickness | 12.7 microns | 0.500 mil |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 60 | 60 | 200 g load |
| Tensile Strength, Ultimate | 290 MPa | 42000 psi | Transverse |
| 300 MPa | 43500 psi | Longitudinal | |
| Elongation at Break | 6.0 % | 6.0 % | Longitudinal |
| 6.0 % | 6.0 % | Transverse |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | <= 0.010 % | <= 0.010 % | |
| Chromium, Cr | <= 0.010 % | <= 0.010 % | |
| Cobalt, Co | <= 0.010 % | <= 0.010 % | |
| Copper, Cu | <= 0.010 % | <= 0.010 % | |
| Iron, Fe | <= 0.010 % | <= 0.010 % | |
| Nickel, Ni | >= 99.95 % | >= 99.95 % | |
| Sulfur, S | <= 0.0020 % | <= 0.0020 % | |
| Zinc, Zn | <= 0.0010 % | <= 0.0010 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00000800 ohm-cm | 0.00000800 ohm-cm |