Material Notes:
Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and impact resistance over conventional homopolymer films.Slip/Antiblock - FINA 6573XHC is formulated with no slip and high antiblock for specialized film handling.FDA - FINA 6573XHC complies with all applicable FDA regulations for food contact applications.Recommended Applications - FINA 6573XHC is recommended for use in manufacture of packaging films that require improved optical and impact properties.Processing - FINA 6573XHC resin processes with typical melt temperatures of 450-525°F (232-274°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Water Vapor Transmission 11.0 g/m²/day

@Temperature 37.8 °C
0.708 g/100 in²/day

@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Melt Flow 8.0 g/10 min
8.0 g/10 min
Conditions not specified; ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 500 %
500 %
Non-oriented film; ASTM D882
Secant Modulus 0.690 GPa
100 ksi
1% Secant Modulus; Non-oriented Film; ASTM D882
Dart Drop 1.40 g/micron
35.6 g/mil
F<sub>50</sub>; ASTM D 1709
Film Tensile Strength at Break, MD 48.3 MPa
7010 psi
Non-oriented film; ASTM D882
Thermal Properties Metric English Comments
Melting Point 148 °C
298 °F
DSC
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
Non-oriented film; ASTM D1003
Gloss 75 %
75 %
45°; Non-oriented film; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 232 - 274 °C
450 - 525 °F