Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer Toyobo
Trade Name VYLOPET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemical & weather resistance, and processability.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Tensile Strength, Ultimate 135 MPa
19600 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 206 MPa
29900 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Compressive Yield Strength 103 MPa
14900 psi
ASTM D695
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 28
28
ASTM D1044
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL-746B
Flammability, UL94 V-0

@Thickness 0.907 mm
V-0

@Thickness 0.0357 in
UL-94
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 24.0 kV/mm

@Thickness 2.00 mm
610 kV/in

@Thickness 0.0787 in
ASTM D149
Arc Resistance 85 sec
85 sec
ASTM D495
Comparative Tracking Index 220 V
220 V
IEC test