Material Notes:
Universal No. 12 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme abrasion and corrosion resistance with moderate impact. The deposited hardness range of Rc 48 - 52 remains intact under operating temperatures of 1500°F. The excellent resistance to hot and cold abrasion, corrosion and erosion suits Universal 12 to numerous applications.Universal No. 12 applications include: rocker arms, trimming dies, mixers, cutters, extrusion and conveyer screws, seats and valves for oil and gas, chipper knives, paper rolls, bushings, saw teeth, entry guides, shafts, shaft bearings, thrust washers, brake drums, tappets, valve push rods and valve stem ends.Machinability: Carbide tools or grinding.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Physical Properties Metric English Comments
Density 8.66 g/cc
0.313 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 48 - 52
48 - 52
Tensile Strength, Ultimate 524 MPa
76000 psi
Compressive Strength 1330 MPa
193000 psi
Thermal Properties Metric English Comments
Melting Point 1260 °C
2300 °F
Maximum Service Temperature, Air 816 °C
1500 °F
Component Elements Properties Metric English Comments
Carbon, C 1.65 %
1.65 %
Chromium, Cr 28.5 %
28.5 %
Cobalt, Co 55.4 - 56.4 %
55.4 - 56.4 %
As Remainder
Iron, Fe 2.0 %
2.0 %
Molybdenum, Mo <= 1.0 %
<= 1.0 %
Nickel, Ni 2.0 %
2.0 %
Silicon, Si 1.0 %
1.0 %
Tungsten, W 8.5 %
8.5 %
Users viewing this material also viewed the following: