Wellman Wellamid® MRGF25/15 22H-NBK1/WE-1364 40% Mineral/Glass Reinforced Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/15 22H-NBK1/WE-1364 40% Mineral/Glass Reinforced Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage, Flow 0.0025 - 0.0065 cm/cm
0.0025 - 0.0065 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 165 MPa
23900 psi
ISO 178-93
Flexural Modulus 8.70 GPa
1260 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-93