Wellman Wellamid® MRGFX1393-N 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGFX1393-N 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Mineral/Glass Reinforced, Silicone Lubricated Nylon 6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183-87
Filler Content 40 %
40 %
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 150 MPa
21800 psi
ISO 178-93
Flexural Modulus 8.20 GPa
1190 ksi
ISO 178-93
Izod Impact, Notched (ISO) 4.90 kJ/m²
2.33 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-93
Flammability, UL94 HB

@Thickness 1.57 mm
HB

@Thickness 0.0618 in