Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate
Manufacturer Westlake Chemical Corporation
Trade Name EMAC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Westlake EMAC® SP2220 is a 20% EMA copolymer designed for compounding, extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficient of friction are required. SP2220 is compatible with and provides excellent adhesion to polyolefins, polyesters, and other polymers while providing outstanding low temperature performance.Applications: films, disposable gloves, tubing and wound care.FDA: This material complies with FDA regulations in 21 CFR, section 177.1340.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM D1505
Methyl Acrylate Content 20 %
20 %
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 36
36
ASTM D2240
Tensile Strength at Break 7.00 MPa
1020 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 675 %
675 %
500mm/min; ASTM D638 Type IV Specimen
Thermal Properties Metric English Comments
Melting Point 82.0 °C
180 °F
by DSC; ASTM D3418
Vicat Softening Point 47.0 °C
117 °F
ASTM D1525
Brittleness Temperature <= -42.0 °C
<= -43.6 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating
Extrusion
Region US & Canada
Bamberger Polymers Distribution