Material Notes:
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical and photographic equipment, valve and pump trim, chemical equipment, digesters, tanks, evaporators, pulp, paper and textile processing equipment and parts exposed to marine atmospheres and tubing.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 862 MPa
>= 125000 psi
Tensile Strength, Yield >= 517 MPa
>= 75000 psi
0.2% Offset
Elongation at Break >= 10 %
>= 10 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.5 µm/m-°C

@Temperature 20.0 - 649 °C
10.3 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 15.9 W/m-K
110 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 16 - 18 %
16 - 18 %
Iron, Fe 62.145 - 72 %
62.145 - 72 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
2.0 - 3.0 %
Nickel, Ni 10 - 14 %
10 - 14 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %