Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Plastcom SLOVALEN PC 63 T 15 PP reinforced with 15% mineral filler Features: Modified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Application in all automotive interior industry.D.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183-1 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Density | 1.01 g/cc @Temperature 23.0 °C |
0.0365 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-2120 17TOP BU is a black colored, 17% talc-filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-2120 17TOP BU is developed for producing injection .. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Density | 1.01 g/cc @Temperature 20.0 °C |
0.0365 lb/in³ @Temperature 68.0 °F |
Relative density |
Suqian Unitechem Light Stabilizer 944 Chemical Name: Poly-{[6-[(1,1,3,3-tetramethylbutyl)amino]-1,3,5-triazine-2,4-diyl][(2,2,6,6-tetramethyl-4-piperidyl)imino]-1,6-hexanediyl[(2,2,6,6-tetramethyl-4-piperidyl)imino]}CAS NO.: 70624-18-9M.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Washington Penn PPC3MF1.5-Black Polypropylene, 15% Mica-Filled, Chemically-Coupled Heat Stabilized injection molding compound. Meets physical requirements for General Motors Spec. GMP.PP.024.Applications: HVAC duct and other various automotive applications.Data provided by Washin.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin.. |
|||
Density | 1.01 g/cc @Temperature 260 °C |
0.0365 lb/in³ @Temperature 500 °F |
Melt |
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | Melt |
Covestro Desmopan® DP 2586A Polyurethane Extrusion- and injection molding gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentBeadsApplicationBlown filmsPreprocessingMax. Water co.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | Melt |
Covestro Desmopan® DP 9395AU Polyurethane Extrusion- and injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood low-temperature flexibilityApplicationPneumatic hosesProfilesCable sheathingsInject.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 16 GM nat PA12 Grilamd L16 GM is a low-viscosity, non-reinforced PA 12 grade, UV- and heat-stabilized. The modification with a crystallization regulator causes a quick freeze and a fine, crystalline structure. Due.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 25H FWA black 9225 PA12 Product Description: Grilamid L 25 H FWA black 9225 is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA black 9225 is designed for technical injection mould.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 3817 black 9992 PA12 Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Arkema Group Orgalloy® LE 60LM Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ISO 1183 |
Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Conditioned) Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High .. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Dry) Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High .. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Buckeye Polymers BP Flex D5606 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | |
BASF AMIX TI Formula: C9H21NO3CAS: 122-20-3Description: AMIX TI is a dark solid that is almost odorless. It is fully soluble in waterSynonyms: TRIPA, 1,1’,1”-Nitrilotri-2-propanol, Tri-2-propanolamine, Tri-is.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | Sintered Part; ASTM D792 |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |
|||
Density | 1.01 g/cc | 0.0365 lb/in³ | ASTM D792 |
Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: BK11 is an SBC consisting of KR03 grade with a mold release added of easier processing. BK11 molded parts give excellent detail on fast production cycl.. |