Material Notes:
Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High thermal and chemical resistance. Outstanding mechanical properties. Low permeability to gas and hydrocarbon.Example applications: Oil tank, hydraulic fluid tank.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 11 %
11 %
50 mm/min
Tensile Modulus 1.08 GPa
157 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 0.670 J/cm²
3.19 ft-lb/in²
0.590 J/cm²

@Temperature -30.0 °C
2.81 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 20.0 °C
55.6 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
Vicat Softening Point 142 °C
288 °F
50°C/hr; 50N
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in
Comparative Tracking Index 600 V
600 V