Material Notes:
Grilamd L16 GM is a low-viscosity, non-reinforced PA 12 grade, UV- and heat-stabilized. The modification with a crystallization regulator causes a quick freeze and a fine, crystalline structure. Due to its good flowability, Grilamid L16 GM is especially suitable for thinwalled injection molding applications.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.400 %
0.400 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 70.0 MPa
10200 psi
conditioned; ISO 2039-1
Tensile Strength at Break 50.0 MPa
7250 psi
dry; ISO 527-1/-2
50.0 MPa
7250 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPa
6530 psi
dry; ISO 527-1/-2
45.0 MPa
6530 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa
160 ksi
conditioned; ISO 527-1/-2
1.50 GPa
218 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
conditioned; ISO 179/1eA
0.500 J/cm²

@Temperature 30.0 °C
2.38 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
140 °C
284 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
conditioned; IEC 60250
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Electricals & Electronics Connectors
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Nucleated
Special Characteristics Improved heat resistance