Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Pyrotek Firefly 800 Roller & Furnace Cladding Material Firefly 800 is a beige asbestos-free material made from high-quality shot-free mineral wool and inert fillers. Rollers made of Firefly 800 are constructed to resist breakage in handling service. F.. |
|||
Density | 0.875 - 2.24 g/cc | 0.0316 - 0.0809 lb/in³ | Average value: 1.11 g/cc Grade Count:307 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D1475 |
Humiseal 1B12 Acrylic Conformal Coating Humiseal 1B12 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityPasses thermal shock test (MIL-I-46058C)Flammabili.. |
|||
Density | 0.875 - 0.899 g/cc | 0.0316 - 0.0325 lb/in³ | |
Lord Adhesives 7707 n-Butyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Silon Tabond 3042 Impact Modifier for PA Tabond 3042 is a chemically modified Ethylene Copolymer/LLDPE.Information provided by Silon |
|||
Density | 0.874 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 13M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.874 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 46 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Density | 0.875 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 75W-80 Mobilfluid LT Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to.. |
|||
Density | 0.875 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Syncon® 220 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Density | 0.874 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 100 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.874 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 46 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | ASTM D792 |
Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP) AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
Dow AFFINITY™ KC 8852 Polyolefin Elastomer AFFINITY® KC 8852 polyolefin elastomer is an ethylene-octene copolymer as for one sided stretch cling film in industrial collation packaging. It exhibits excellent inherent cling and optics while o.. |
|||
Density | 0.875 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 75W-80 Mobilfluid LT Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to.. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D792 |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Density | 0.875 g/cc @Temperature 15.6 °C |
0.0316 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 46 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Conoco® El Mar® Mid Ash Heavy Duty SAE 30 Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips El Mar® Grade 15W-40 Geo Oil Description: Conoco El Mar® Geo Oil is a high-quality, rust- and oxidation-inhibited, nondetergent, ashless gas engine oil. It is formulated with high viscosity index paraffinic base oils blended w.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® 150 Multipurpose R&O Oil, AGMA Lubricant No. 4 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® 580 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Sulnap® 22 Cutting Oil Description: Conoco Sulnap Cutting Oil is suited for general-purpose machining operations, such as turning, boring, planing, shaping, light- to medium-duty threading, sawing, hobbing and gear cuttin.. |
|||
Density | 0.876 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Hydroclear® MV150 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Density | 0.875 g/cc @Temperature 0.000 °C |
0.0316 lb/in³ @Temperature 32.0 °F |
|
BorsodChem ONGRONOX INP 75 D peroxide-type initiator Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide.Mol. wt: 314.50 g/mol.Active oxygen content: 5.09 %.Deflegmation material: isododecane.Major decomposition products.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Density | 0.876 g/cc @Temperature 15.0 °C |
0.0316 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 46 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.875 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Conoco® El Mar® 15W-40 Mid Ash Heavy Duty Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Density | 0.874 g/cc | 0.0316 lb/in³ | |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |