Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183 |
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization packageCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use stra.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Cast/Blown Film ResinCharacteristics: Good Drawdown, Can be used in blown or cast applicationsApplications:Stretch Wrap, CoextrusionsProcessing Conditions: Extruder 6.3.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
ExxonMobil Exceed™ 2018CA Blown Film Resin
(discontinued **) Exceed 2018CA resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals EXXPOL® Technology. The higher melt index makes this polymer ideally sui.. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D792 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-21 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-23 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA942094 Low Density Polyethylene ApplicationsPETROTHENE NA 942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone, and agricultural and c.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake EF603 Low Density Polyethylene Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake EM1870AA Low Density Polyethylene WESTLAKE low-density polyethylene EM1870 is used for injection molding applications. It has excellent stress crack resistance for lids.Application/UsesFlexible medicalLidsMedicalFDA: This material c.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake LF2050 Hexene Linear Low Density Polyethylene Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183 |
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear.. |
|||
Density | 0.920 - 0.940 g/cc | 0.0332 - 0.0340 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTALENE EN 10 SC Modified Polyolefin Blend Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05HH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 2018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018CA is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coex.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Bapolene® 122F Polyethylene, Film Grade Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. .. |
|||
Density | 0.920 g/cc | 0.0332 lb/in³ | ISO 1183 |
CENTROPLAST CENTROLEN PPS Polypropylene flame resistant This material is a low density, easily machined plastic that can be welded and is flame resistant. Applications include exhaust systems for heating systems, and apparatus engineering.Information pr.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
M. Holland Company LD220MM LDPE
(discontinued **) Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | base resin; ISO 1183 |
Borealis LE6022 Polyethylene Modified Jacketing Compound LE6022 is a black low density copolymer modified polyethylene compound. It is characterized by excellent crack resistance and mechanical properties and low temperature performance in combination wit.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | |
LyondellBasell Lupolen® 1800 H LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |