Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183-A |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | NCMT Method |
NCMT NanoPAC™ G1000 High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH TS15010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 0.960 - 0.964 g/cc | 0.0347 - 0.0348 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 2062U (62111) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183-1 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 19H Homopolymer HDPE Film Resin Features: High stiffnessGood processability Low gel Applications: BlendingCo-extrusionInformation provided by Nova Chemicals |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Petromont 2200 High Density Polyethylene Resin Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring impr.. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Petromont 8001 High Density Polyethylene Resin Pétromont HDPE 8001 is a high density, homopolymer polyethylene resin produced using the UNIPOL® Process. This high strength resin is intended for extrusion on cast line, where excellent processab.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | |
Mitsui Fybrel® E 400 Polyolefin Synthetic Pulp, Wet Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D-792 |
Polyram BondyRam® 2001 Maleic Anhydride modified EVA coupling agent
(discontinued **) Maleic Anhydride Modified grafted EVA (28%VA) recommended as adhesive promoter and general purpose compatibilizerInformation provided by Polyram Ram On Ind. |
|||
Density | 0.960 - 1.30 g/cc | 0.0347 - 0.0470 lb/in³ | Average value: 1.05 g/cc Grade Count:13 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
LyondellBasell Alathon® M6060 High Density Polyethylene ApplicationsALATHON M 6060 is a medium molecular weight high density homopolymer with extremely low gel content. This resin provides high stiffness and narrow molecular weight distribution for use .. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM D4883 |
Ineos T60-800 HDPE Ineos T60-800 is a high density polyethylene homopolymer. This narrow molecular weight distribution resin is a product of Ineos' innovative technology. Parts fabricated from this material exhibit .. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
DuPont Bynel® 3860 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® K605 HDPE Blow Molding Resin Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional rigidityExcellent melt strengthApplications: Automotive bumper beamsInformation provided by Chevron Phillips. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Density | 0.960 g/cc @Temperature 23.0 °C |
0.0347 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 18 MA 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 18 MA 02 is a polymer of .. |
|||
Density | 0.961 g/cc | 0.0347 lb/in³ | ASTM-D792 |
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0334G10CL Glass Reinforced Coupled |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0334M10CL Mica Reinforced Coupled |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Buckeye Polymers BP Flex A9008 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Density | 0.960 g/cc @Temperature 23.0 °C |
0.0347 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group EVATANE® 33-400 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-400 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-400 is stabilized with antioxidants. The High Vinyl Acetate .. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Aclo Accuguard Polypropylene CP0467V2CSL Copolymer Flame Retardant Copper Stabilized |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
Buckeye Polymers BP Flex D0840 TPO Replace Flex PVCTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resis.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFLEX E 75.1 TPE-V, Shore A75 TPE-VInformation provided by BARLOG plastics GmbH. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2915 HDPE Injection Molding Resin
(discontinued **) Features: Excellent balance of stiffness and toughness, low odor, permits light weight container design.Applications: Thin walled food containers, frozen food containers.Data provided by the manufac.. |
|||
Density | 0.960 - 0.960 g/cc @Temperature 290 - 290 °C |
0.0347 - 0.0347 lb/in³ @Temperature 554 - 554 °F |
Average value: 0.960 g/cc Grade Count:1 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 0.960 g/cc | 0.0347 lb/in³ | ISO 1183/A |
Addiplast Addilene PMD 50265 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |