Density >= 0.0350 g/cc
>= 0.00126 lb/in³
Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure
NOVA Chemicals Dytherm® 370R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0350 - 0.100 g/cc
0.00126 - 0.00361 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
NOVA Chemicals Dytherm® 370R Expandable Polystyrene
This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma..
Density 0.0350 g/cc
0.00126 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0350 g/cc
0.00126 lb/in³
Zircar Ceramics Alumina Mat
A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between..
Density 0.0350 g/cc
0.00126 lb/in³
Dow Styrofoam™ Polystyrene Rigid Foam Insulation
The information below is typical of Styrofoam™ rigid polystyrene foam used for construction insulation - but many specific grades are available. This material is produced as sheets of closed-cell ..
Density 0.0350 g/cc
0.00126 lb/in³
Brandenburger ISOFLEX AFV Foam
This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio..
Density 0.0350 g/cc
0.00126 lb/in³
BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe)
Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e..
Density 0.0350 g/cc
0.00126 lb/in³
ISO 845
BASF Neopolen® P 9035 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Density 0.0350 g/cc
0.00126 lb/in³
ISO 845
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Density 0.0350 g/cc
0.00126 lb/in³
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Density 0.0350 g/cc
0.00126 lb/in³
ISO 845
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Density 0.0350 g/cc
0.00126 lb/in³
ISO 845
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..