Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0350 g/cc | >= 0.00126 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 370R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0350 - 0.100 g/cc | 0.00126 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 370R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | |
Dow Styrofoam™ Polystyrene Rigid Foam Insulation The information below is typical of Styrofoam™ rigid polystyrene foam used for construction insulation - but many specific grades are available. This material is produced as sheets of closed-cell .. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | |
Brandenburger ISOFLEX AFV Foam This material is a noncombustible, inorganic, flexible insulating foam used as exterior lining to save thermal energy, mainly in the rubber and plastics industry. It is also used in the refrigeratio.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | |
BASF E-por® 0.035 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | ISO 845 |
BASF Neopolen® P 9035 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | ISO 845 |
BASF Neopolen® P 9335 MG 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | ISO 845 |
BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Density | 0.0350 g/cc | 0.00126 lb/in³ | ISO 845 |
BASF Neopolen® P 9435 0.035 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |