Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON ICE 504L PPS, 40% Specialty
(Unverified Data**) FORTRON ICE 504L is a 40% glass fiber reinforced material that belongs to our new generation of PPS. This new technology allows optimization of molding conditions with faster cycle times for complex.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Density | 1.65 - 1.75 g/cc | 0.0596 - 0.0632 lb/in³ | ASTM D792 |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-220BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications requiring .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
(Unverified Data**) Fortron 1140L0 is a 40% glass-reinforced extrusion grade. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently flame-retardant. The high hardness and rig.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced
(Unverified Data**) One of the easiest flowing 40% glass reinforced grade in the Fortron product line. This material can be processed at fast cycle times due to the unique crystallization characteristics. This product .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | |
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFL25 Acetal Copolymer LNP LUBRICOMP* KFL25 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® V9290 PET (Europe-Africa-Middle East) 45% GF PET, Glass, Mold Release, Heat Stabilized, |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PBT GB30 TL15 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear (Europe-Africa-Middle East) LNP* Thermocomp* OF008 is a compound based on PPS - Linear resin containing Glass Fiber. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | D792 |
Zhejiang Juner 301-G30 30% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792-91 |
Engineered Polymer Solutions PET 5300 FR, 30% Glass Filled Natural and colors available. Injection molding grade. Uses: General Purpose, pump housings, electricalInformation provided by Engineered Polymer Solutions. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON MT9141L4 DW PPS, 40% Specialty Fortron MT9141L4 DW is a 40% glass-reinforced PPS that has excellent heat and chemical resistance, inherently flame-retardant, high hardness and a good balance of strength and stiffness. This grade .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | |
BASF Paliogen® Red L 3885 Color Additive Description: Transparent perylene red with a very clean shadSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Airdrying syste.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON ICE 506L PPS, 40% Glass Reinforced Fortron ICE 506L is a faster crystallizing version of Fortron 1140L6. It offers essentially the same characteristics of 1140L6 with improved crystallization efficiency for faster cycle times in comp.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese VECTRA A530 LCP, 30% Mineral Reinforced Best overall surface appearance with properties similar to A130. Less abrasive than glass fiber reinforced grades. Improved toughness over A130. Outstanding hydrolytic stability. Recommended wher.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON MT9140L6 PPS, 40% Medical Technology
(Unverified Data**) Fortron MT9140L6 is a 40% glass fiber reinforced injection molding grade with a low melt viscosity. It exhibits excellent heat and chemical resistance, inherent flame retardancy and shows high hardn.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RVL29XXP PA 66 (Europe-Africa-Middle East) LNP VERTON* RVL29XXP is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS) Description: Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grad.. |