Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp OFP36A PPS - Branched LNP LUBRICOMP* OFP36A is a compound based on PPS - Branched resin containing Glass Fiber, Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SA.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. |
|||
Density | 1.65 g/cc @Temperature 25.0 °C |
0.0596 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® SV55 PFPE Solvent Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF0069RS PA 66 LNP THERMOCOMP* RF0069RS is a compound based on Nylon 66 resin containing Glass Fiber, Mold Release, Flame Retardant. Added features of this material include: Easy Release.This data was supplied by.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Tipco Tipcolite® THD 111 Phenolic Compound, Short Glass Fibers & Minerals, Medium -Soft Flow & High Strength Medium -Soft Flow Phenolic Compound, Reinforced with Short Glass Fibres & MineralsApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, T.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | DIN 53 479 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE15022 NC010 Polyethylene Terephthalate (PET) 36% Glass Reinforced Polyethylene TerephthalateRynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performan.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792-91 |
Engineered Polymer Solutions PET 5300 FR, 30% Glass Filled Natural and colors available. Injection molding grade. Uses: General Purpose, pump housings, electricalInformation provided by Engineered Polymer Solutions. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Celanese Celanex® 6400 Polyester (PBT), 40% Glass/Mineral Warp resistant, good surface smoothnessInformation provided by Celanese Corporation. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON® 9140L4 40% Glass Reinforced Polyphenylene Sulfide (PPS) Description: Fortron 9140L4 is a 40% glass fiber reinforced injection molding grade that exhibits excellent heat and chemical resistance, inherent flame retardancy, and high hardness and rigidity at.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | |
BASF Paliogen® Red L 3885 Color Additive Description: Transparent perylene red with a very clean shadSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Airdrying syste.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON MT9140L6 PPS, 40% Medical Technology Fortron MT9140L6 is a 40% glass fiber reinforced injection molding grade with a low melt viscosity. It exhibits excellent heat and chemical resistance, inherent flame retardancy and shows high hardn.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® 301-G30 PBT Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | Coating on BOPP |
Solvay Specialty Polymers Diofan® A 036 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® A 036 is a PVDC latex used as a flexible under layer for coating on paper and cardboard, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYING - DIOFAN® A 0.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese Coolpoly® D3606 Thermally Conductive Polyamide 4,6
(discontinued **) CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X611 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | DIN 53 47 |
Albis Plastics Tedur® L 9510-1 PPS, 40% Glass Fiber High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Impellers, Valve Housings and BushingsProcessing: Injection Molding (.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON MT9140L6 PPS, 40% Medical Technology
(Unverified Data**) Fortron MT9140L6 is a 40% glass fiber reinforced injection molding grade with a low melt viscosity. It exhibits excellent heat and chemical resistance, inherent flame retardancy and shows high hardn.. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese FORTRON MT9141L4 DW PPS, 40% Specialty
(Unverified Data**) Fortron MT9141L4 DW is a 40% glass-reinforced PPS that has excellent heat and chemical resistance, inherently flame-retardant, high hardness and a good balance of strength and stiffness. This grade .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
DSM Arnite® TV4 260 SF PBT-30% Glass Reinforced (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | dry; ISO 1183 |
DSM Novamid® MC112LG55 C10 PA6-GF55 55% Glass Reinforced |
|||
Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced Super High Flow, High heat Resistance and Low Warp for Thin Parts.Information provided by Celanese |