Physical Properties Metric English Comments
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/16" to 1/4"
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/8" to 1"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8"
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1"