Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Bedford Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1".pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many chemicalsLight Weight- Weighs nearly 80% less than a steel profile of similar dimensionElectrically Non-ConductiveNon-MetallicLower Life Cycle CostNon-Leaching. Environmentally FriendlyDimensional StabilityInformation provided by Bedford Plastics.
Physical Properties Metric English Comments
Density 1.72 - 1.94 g/cc
0.0620 - 0.0700 lb/in³
ASTM D792
Water Absorption <= 0.60 %
<= 0.60 %
24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 40
40
ASTM D2583
Tensile Strength, Ultimate 68.9 MPa
10000 psi
Crosswise; ASTM D638
165 MPa
24000 psi
Lengthwise; ASTM D638
Tensile Modulus 9.65 GPa
1400 ksi
Crosswise; ASTM D638
13.8 GPa
2000 ksi
Lengthwise; ASTM D638
Flexural Strength 124 MPa
18000 psi
Crosswise; ASTM D790
207 MPa
30000 psi
Lengthwise; ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
Crosswise; ASTM D790
13.8 GPa
2000 ksi
Lengthwise; ASTM D790
Compressive Strength 114 MPa
16500 psi
Crosswise; ASTM D635
165 MPa
24000 psi
Lengthwise; ASTM D635
Compressive Modulus 6.89 GPa
1000 ksi
Crosswise; ASTM D635
12.4 GPa
1800 ksi
Lengthwise; ASTM D635
Ultimate Bearing Strength 221 MPa
32000 psi
Lengthwise; ASTM D953
Shear Strength 41.4 MPa
6000 psi
Perpendicular Shear Stress, Lengthwise; ASTM D3946
41.4 MPa
6000 psi
Perpendicular Shear Stress, Crosswise; ASTM D3946
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
Crosswise; ASTM D256
10.7 J/cm
20.0 ft-lb/in
Lengthwise; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 8.00 µm/m-°C

@Temperature 20.0 °C
4.44 µin/in-°F

@Temperature 68.0 °F
Lengthwise; ASTM D696
Flammability, UL94 V-0
V-0
Flame Spread Index <= 25
<= 25
Tunnel Test; ASTM E84
NBS Smoke Density 600 - 700
600 - 700
ASTM E662
Electrical Properties Metric English Comments
Dielectric Strength 1.38 kV/mm
35.0 kV/in
Lengthwise; ASTM D149
7.87 kV/mm
200 kV/in
Perpendicular to Laminate Face; ASTM D149
Arc Resistance 120 sec
120 sec
Lengthwise; ASTM D495
Descriptive Properties Value Comments
Flammability Nonburning
ASTM D635